FIELD: chemistry.
SUBSTANCE: method involves electro-plasma spraying of alumina powder having a particle size of 50-100 mcm on a product surface at a spraying distance from 100 to 120 mm at arc current 300 to 350 A and anodic micro-arc oxide coating at current density (1-2)×103 A/m2, for 10 to 30 minutes in a sodium hydroxide alkaline electrolyte in an amount of 1-3 g/l.
EFFECT: improved mechanical properties of plasma-sprayed coatings on titanium and its alloys, particularly micro-hardness and reduced time of coating deposition.
2 dwg, 2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FORMING CERAMIC COATING BASED ON ZIRCONIUM DIOXIDE ON ARTICLE FROM TITANIUM ALLOY | 2015 |
|
RU2607390C2 |
METHOD FOR PREPARING LANTHANUM-CONTAINING COATING | 2012 |
|
RU2494764C1 |
METHOD FOR FORMING METAL OXIDE POROUS COATINGS ON TITANIUM PRODUCTS | 2022 |
|
RU2781873C1 |
METHOD OF MANUFACTURING INTRAOSSEOUS IMPLANTS WITH MULTI-LAYERED COATING | 2013 |
|
RU2526252C1 |
METHOD OF MANUFACTURING INTRAOSSEOUS DENTAL IMPLANT | 2013 |
|
RU2525737C1 |
METHOD FOR ELECTROPLASMA SPATTERING OF BIOCOMPATIBLE COATINGS BASED ON MAGNESIUM-CONTAINING TRICALCIUM PHOSPHATE | 2016 |
|
RU2641597C1 |
METHOD OF PRODUCING BIOCOMPATIBLE COATING ON BASIS OF MAGNESIUM-SUBSTITUTED HYDROXYAPATITE | 2015 |
|
RU2604134C1 |
METHOD OF TITANIUM POROUS COATINGS FORMING ON TITANIUM IMPLANTS | 2017 |
|
RU2647968C1 |
METHOD OF SPUTTERING BIOCOMPATIBLE COATING MODIFIED WITH LOW DECOMPOSITION TEMPERATURE COMPONENT | 2018 |
|
RU2684283C1 |
METHOD FOR MAKING BIOACTIVE COATED ENDOSSEOUS IMPLANT | 2013 |
|
RU2530573C1 |
Authors
Dates
2015-11-10—Published
2014-05-19—Filed