FIELD: electricity.
SUBSTANCE: reservoir for hydrogen storage represents a regular nickel-cadmium accumulator with metal ceramic electrodes. The proposed hydrogen accumulation method consists in saturation of metal ceramic electrodes with hydrogen by means of its diffusion inside electrodes. Electrodes are saturated with hydrogen, due to electrolysis of electrolyte during accumulator recharge under voltage of 1.5 V for 2 years.
EFFECT: possibility to use cheap commercial metal ceramic electrodes for hydrogen accumulation and production of mass hydrogen content in oxide-nickel electrodes of 13,4, and in cadmium electrodes of 8 percent.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HYDROGEN RECOVERY FROM METAL HYDRIDE | 2017 |
|
RU2671322C1 |
METHOD OF BLOCKING NICKEL-CADMIUM BATTERY THERMAL RUNAWAY | 2017 |
|
RU2659797C1 |
METHOD OF CREATING NICKEL-CADMIUM ACCUMULATORS WITH CERMET ELECTRODES, NOT SUBJECT TO HEAT OVERCLOCKING | 2016 |
|
RU2617687C1 |
METHOD FOR REDUCING THE HEAT RATE COEFFICIENT IN THE NICKEL-CADMIUM BATTERY BY MEANS OF VARIABLE ASYMMETRIC CURRENT | 2016 |
|
RU2658859C2 |
METHOD OF HYDROGEN ACCUMULATION | 2012 |
|
RU2515971C2 |
METHOD OF HYDROGEN ACCUMULATION IN LAMELLAR ELECTRODES | 2014 |
|
RU2573439C1 |
METHOD FOR RESTORATION OF NICKEL-CADMIUM BATTERIES WITH ASYMMETRIC ALTERNATING CURRENT | 2012 |
|
RU2527937C2 |
METHOD FOR ACCELERATED BUILD-UP AND RECOVERY OF CAPACITY FOR NICKEL-CADMIUM ACCUMULATORS BY ALTERNATING ASYMMETRIC CURRENT | 2012 |
|
RU2521607C1 |
METHOD OF MANUFACTURING THE BASIS OF THE ELECTRODE OF A CHEMICAL SOURCE OF A CURRENT FROM A CARBON TISSUE USING A VARIABLE ASYMMETRIC CURRENT | 2017 |
|
RU2672854C1 |
DEVICE FOR ANALYSING SUSCEPTIBILITY OF NICKEL-CADMIUM ACCUMULATOR TO HEAT ACCELERATION | 2009 |
|
RU2390886C1 |
Authors
Dates
2016-01-20—Published
2014-07-31—Filed