FIELD: electricity.
SUBSTANCE: manufacturing nickel-cadmium accumulators with cermet electrodes includes the following stages: manufacturing a cermet electrode base, impregnating negative and positive electrodes with appropriate active substances, placing the electrodes in the separators and accumulator assembly, placing the cermet oxide-nickel electrodes in bags of thin nickel perforated foil with the thickness of 2-5 mcm (before the stage of placing the electrodes in the separators), wherein at the top the foil bags are welded to the current leads of the electrodes.
EFFECT: invention allows to create a nickel-cadmium accumulator with cermet electrodes, that is not subjected to heat overclocking.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF BLOCKING NICKEL-CADMIUM BATTERY THERMAL RUNAWAY | 2017 |
|
RU2659797C1 |
METHOD OF HYDROGEN RECOVERY FROM METAL HYDRIDE | 2017 |
|
RU2671322C1 |
METHOD OF HYDROGEN ACCUMULATION IN METAL CERAMIC ELECTRODES | 2014 |
|
RU2573544C1 |
METHOD FOR REDUCING THE HEAT RATE COEFFICIENT IN THE NICKEL-CADMIUM BATTERY BY MEANS OF VARIABLE ASYMMETRIC CURRENT | 2016 |
|
RU2658859C2 |
METHOD OF HYDROGEN ACCUMULATION IN LAMELLAR ELECTRODES | 2014 |
|
RU2573439C1 |
METHOD OF HYDROGEN ACCUMULATION | 2012 |
|
RU2515971C2 |
DEVICE FOR ANALYSING SUSCEPTIBILITY OF NICKEL-CADMIUM ACCUMULATOR TO HEAT ACCELERATION | 2009 |
|
RU2390886C1 |
METHOD FOR RESTORATION OF NICKEL-CADMIUM BATTERIES WITH ASYMMETRIC ALTERNATING CURRENT | 2012 |
|
RU2527937C2 |
METHOD OF MANUFACTURING THE BASIS OF THE ELECTRODE OF A CHEMICAL SOURCE OF A CURRENT FROM A CARBON TISSUE USING A VARIABLE ASYMMETRIC CURRENT | 2017 |
|
RU2672854C1 |
METHOD FOR ACCELERATED BUILD-UP AND RECOVERY OF CAPACITY FOR NICKEL-CADMIUM ACCUMULATORS BY ALTERNATING ASYMMETRIC CURRENT | 2012 |
|
RU2521607C1 |
Authors
Dates
2017-04-26—Published
2016-10-18—Filed