FIELD: metal processing.
SUBSTANCE: invention relates to a method of pressure welding of metal parts and can be used in machine building. Welded parts are compressed. Welding zone is heated to temperature lower than recrystallisation temperature on one side of contact zone with movement of temperature field through contact zone. Welding is carried out. After welding isothermal holding at temperature higher threshold of recrystallisation is carried out.
EFFECT: heating for isothermic curing is performed on one side of contact zone with displacement of recrystallisation front through contact zone.
1 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PRESSURE WELDING WITH HEATING | 2016 |
|
RU2641215C2 |
CONTACT SEAM WELDING METHOD | 2018 |
|
RU2706264C1 |
0 |
|
SU551139A1 | |
METHOD OF ELECTRIC SURFACE WELDING | 1996 |
|
RU2104845C1 |
ELECTRIC-RESISTANCE FUSION ON METHOD | 1997 |
|
RU2122928C1 |
PROCEDURE FOR TREATMENT OF SEMI-FINISHED PRODUCT OUT OF LOW ALLOYED DISPERSE-HARDENING COPPER ALLOY WITH CONTENTS OF NICKEL TO 1,6 %, BERRILIUM 0,2-0,8 % AND TITANIUM TO 0,15 % | 2009 |
|
RU2416672C1 |
METHOD FOR OBTAINING METAL POWDER FROM TOOL STEEL WASTE IN WATER | 2022 |
|
RU2791308C1 |
METHOD FOR MANUFACTURING A COMPOSITE WORKPIECE OF "DISC-SHAFT" TYPE FROM HEAT-RESISTANT ALLOYS | 2019 |
|
RU2706925C1 |
METHOD OF WELDING BY APPLICATION OF PRESSURE AND HEAT | 0 |
|
SU1151404A1 |
METHOD OF DIFFUSION WELDING | 0 |
|
SU1602651A1 |
Authors
Dates
2016-07-10—Published
2014-11-21—Filed