FIELD: metallurgy.
SUBSTANCE: method includes electrolytic coating deposition in electrolyte containing, g/l: copper (II) borofluoride (in terms of metal) 55-70, tin (II) borftluoride (in terms of metal) 40-45, boron fluoride 110- 200, boric acid 40-100, antioxidant 4-10, surfactant 0.5-2.5, at a cathode current density of 2.0-10.0 A/dm2 and electrolyte temperature 18-25°C.
EFFECT: increased abrasion and corrosion resistance of the coating under conditions of fretting corrosion, reduced friction coefficient, increased hardness, wear resistance and thermal stability of the coating.
3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ELECTROLYTIC DEPOSITION OF CORROSION-RESISTANT ANTIFRICTION COATINGS BY THE COPPER ALLOY | 2016 |
|
RU2620215C1 |
ACID ELECTROLYTE FOR APPLICATION OF ANTIFRICTION COATING WITH LEAD-TIN-COPPER ALLOY | 2020 |
|
RU2739899C1 |
ELECTROLYTE FOR APPLYING ANTI-FRICTION COATINGS | 2023 |
|
RU2820009C1 |
SLIDING ELEMENT | 2018 |
|
RU2712496C1 |
SELECTIVE ETCHER OF MULTI-COMPOSITE ELECTROLYTIC COATINGS BASED ON TIN AND LEAD | 2018 |
|
RU2690871C1 |
METHOD FOR PRODUCING TIN-INDIUM ALLOY COATED COPPER WIRE | 2021 |
|
RU2764277C1 |
METHOD FOR PRODUCING TIN-INDIUM ALLOY COATED COPPER WIRE | 2021 |
|
RU2764274C1 |
METHOD FOR PRODUCING COPPER WIRE COATED ON THE BASIS OF AN ALLOY OF TIN-INDIUM | 2021 |
|
RU2768620C1 |
MULTI-LAYER CRANKSHAFT CONNECTING ROD BEARING | 2023 |
|
RU2813220C1 |
METHOD OF COATING STEEL PARTS | 1993 |
|
RU2103424C1 |
Authors
Dates
2017-05-11—Published
2016-05-31—Filed