FIELD: metallurgy.
SUBSTANCE: rod is produced by rolling an aluminium plate to a thickness of 0.2-0.3 mm, recrystallization of the obtained aluminium strip at a temperature of 200-300°C, applying a friable modifier based on nanocarbon on it and then pressing the strip with a modifier into the bar.
EFFECT: invention makes it possible to improve the mastering of the alloy modifier and thereby improve the mechanical and performance characteristics of castings made from these alloys by reducing the dimensions of aluminium dendrites, αsolid solution, eutectic and primary silicon crystals.
4 dwg
Title | Year | Author | Number |
---|---|---|---|
MODIFICATION METHOD OF ALUMINIUM AND ALUMINIUM-SILICONE ALLOYS (SILUMINS) BY CARBON | 2013 |
|
RU2538850C2 |
METHOD OF MAKING CONDITIONING AGENT FOR HYPOEUTECTIC ALUMINIUM-SILICON ALLOYS | 2011 |
|
RU2475334C2 |
SCHUNGITE AS MODIFIER FOR ALUMINIUM-SILICON ALLOYS | 2015 |
|
RU2609109C1 |
MODIFICATION METHOD OF ALUMINIUM-SILICON ALLOYS | 2015 |
|
RU2623966C2 |
Method for modifying aluminum-silicon alloys | 2020 |
|
RU2743945C1 |
PRODUCTION OF MODIFIER FOR ALUMINIUM ALLOYS | 2013 |
|
RU2528598C1 |
MODIFIER FOR ALUMINIUM ALLOYS | 0 |
|
SU1057161A1 |
METHOD OF PRODUCTION OF BLANKS OUT OF ALUMINIUM-SILICON ALLOYS | 2006 |
|
RU2334588C1 |
MODIFICATION METHOD OF ALUMINIUM-SILICON ALLOYS | 2011 |
|
RU2475550C1 |
METHOD OF BASE METAL PRODUCTION FOR ALUMINIUM ALLOYS | 2013 |
|
RU2533245C1 |
Authors
Dates
2017-07-03—Published
2015-11-10—Filed