FIELD: chemistry.
SUBSTANCE: nepheline raw materials are ground, sintered at a temperature of 400-1000°C with sodium carbonate, or potassium disulfate, or potassium hydrogen sulfate. Speck is treated with water, or an aqueous solution of sulfuric or hydrochloric acid, or an aqueous solution of titanium chloride to obtain a liquid silica-alumina coagulant.
EFFECT: lower costs.
2 cl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING ALUMOSILICON FLOCCULANT-COAGULANT | 2015 |
|
RU2588535C1 |
METHOD OF PRODUCING COMPLEX ALUMINIUM-CONTAINING COAGULANT | 2019 |
|
RU2720790C1 |
METHOD FOR OBTAINING REAGENT FOR WATER PURIFICATION | 2022 |
|
RU2785095C1 |
METHOD FOR OBTAINING A COMPLEX ALUMINUM-CONTAINING COAGULANT | 2021 |
|
RU2761205C1 |
METHOD OF PRODUCING ALUMOSILICIC COAGULANT-FLOCCULANT | 2009 |
|
RU2421400C1 |
METHOD FOR PRODUCING COAGULANT BASED ON ALUMINIUM POLYOXYSULFATE, COAGULANT PRODUCED BY SAID METHOD | 2015 |
|
RU2617155C1 |
NEPHELINE COAGULANT | 2005 |
|
RU2283286C1 |
METHOD FOR INDUSTRIAL SEWAGE TREATMENT | 1993 |
|
RU2049735C1 |
METHOD OF OBTAINING ALUMOSILICON FLOCCULANT-COAGULANT AND WATER PURIFICATION METHOD USING SAID FLOCCULANT-COAGULANT | 2008 |
|
RU2388693C2 |
METHOD FOR PROCESSING SYNNYRITE | 2020 |
|
RU2753109C1 |
Authors
Dates
2017-07-03—Published
2016-09-29—Filed