FIELD: pharmacology.
SUBSTANCE: to produce hydroxyapatite Ca10(PO4)6(HE)2, 0.2 M solution of ethylenediamine succinic acid is added to an aqueous solution of calcium nitrate at room temperature. An aqueous solution of monoammonium phosphate is added to this mixture, dropwise, at constant stirring. The precipitate is aged for 1 day, filtered and dried.
EFFECT: invention allows to obtain an environmentally friendly product with minimal power consumption and raw material costs.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING HYDROXYAPATITE | 2008 |
|
RU2391117C1 |
METHOD OF PRODUCING NANOSIZED HYDROXYAPATITE POWDER | 2011 |
|
RU2457174C1 |
METHOD OF OBTAINING SILICON-MODIFIED HYDROXYAPATITE WITH APPLICATION OF SHF-RADIATION | 2012 |
|
RU2507151C1 |
METHOD OF PRODUCING NANOSIZED HYDROXYAPATITE | 2020 |
|
RU2736048C1 |
METHOD FOR OBTAINING MAGNESIUM-SUBSTITUTED HYDROXYAPATITE | 2015 |
|
RU2617103C1 |
METHOD FOR PRODUCING BIOACTIVE HYDROXYAPATITE | 2015 |
|
RU2604411C1 |
ELECTROLYTE FOR DEPOSITING COATING FROM COPPER-INDIUM ALLOY | 2017 |
|
RU2665855C1 |
AMORPHOUS CARBONIZED AND FLUORINATED HYDROXYAPATITE FOR TOOTH PASTE AND METHOD FOR ITS OBTAINING | 1999 |
|
RU2179437C2 |
METHOD OF OBTAINING COMPOSITION SORBENT | 2018 |
|
RU2675866C1 |
METHOD OF CLEANING SUBJECT SURFACE, MADE OF NOBLE METALS | 2016 |
|
RU2631229C1 |
Authors
Dates
2018-01-23—Published
2016-12-20—Filed