FIELD: chemical-thermal treatment.
SUBSTANCE: to improve tribological properties of nitrided steel articles, the method of making steel articles involves nitriding (210) of a steel article at nitrification temperature in range of 350–650 °C to obtain a nitrided steel article. Nitrided steel items are hardened (220) in reactive hardening oil at nitrification temperature. Reactive hardening oil contains at least one of S, P, B, Mo and W. Thus hardening additionally contains coating (222) of nitrated steel item with solid lubricant containing at least one of S, P, B, Mo and W. Also disclosed are a device for making steel articles, hardening oil and a steel article obtained using said method.
EFFECT: disclosed are steel articles coated with solid lubricant, method and device for their production, and hardening oil used in their production.
25 cl, 9 dwg
Title | Year | Author | Number |
---|---|---|---|
NITRIDE-HARDENED SINTERED STEELS | 2011 |
|
RU2559603C2 |
METHOD FOR INCREASING THE WEAR RESISTANCE AND CORROSION RESISTANCE OF AUSTENITIC STEEL PRODUCTS | 2020 |
|
RU2758506C1 |
METHOD OF HEAT-TREATED STEEL PARTS SURFACES HARDENING | 2015 |
|
RU2603932C1 |
METHOD OF MANUFACTURING PARTS FROM PLASTIC, IN PARTICULAR PROFILED PARTS FROM POLYURETHANE | 1997 |
|
RU2201342C2 |
COUPLE OF GUIDE ELEMENTS, ONE OF WHICH IS IMPLEMENTED FROM SPECIAL STEEL, PROVIDING IMPROVEMENT OF STABILITY CHARACTERISTICS AGAINST JAMMING | 2006 |
|
RU2377450C2 |
WELDING MATERIAL FOR WELD CLADDING | 2013 |
|
RU2650367C2 |
STEEL, PRODUCT MADE OF SAID STEEL AND METHOD FOR PRODUCTION THEREOF | 2016 |
|
RU2743570C2 |
STRENGTHENING METHOD OF STEEL PISTON RING SURFACES | 2008 |
|
RU2386726C1 |
METHOD FOR RESTORATION OF STREGTHENED LAYER PARTIALLY REMOVED FROM STEEL PARTS | 2015 |
|
RU2631436C2 |
METHOD FOR CHEMICAL AND HEAT TREATING TOOL STEELS | 0 |
|
SU926070A1 |
Authors
Dates
2020-04-08—Published
2016-10-25—Filed