FIELD: electrical industry.
SUBSTANCE: effect is achieved by increasing dispersion of silver vanadate and increasing the diffusion coefficient of lithium, for which purpose the method involves mixing vanadium pentoxide with silver nitrate in dry form followed by mechanical activation, heat treatment and cooling to the ambient temperature. Mechanical activation is carried out in a planetary mill at a drum rotation speed of 450 rpm for 30 minutes, heat treatment is carried out at a temperature of 700°C for 5 hours. The activated mixture is compressed into tablets. Heating and cooling are carried out at a rate of 5-10°/min.
EFFECT: improved manufacturability of the cathode while increasing its discharge capacity.
1 cl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
LITHIUM BATTERY CATHODE ACTIVE MASS MANUFACTURING METHOD | 2023 |
|
RU2815267C1 |
METHOD OF PRODUCING LITHIUM BATTERY CATHODE ACTIVE MASS | 2020 |
|
RU2738800C1 |
MANUFACTURING METHOD OF ACTIVE MASS OF CATHODE OF LITHIUM CURRENT SOURCE | 2010 |
|
RU2424599C1 |
CATHODE MATERIAL FOR LITHIUM CURRENT SUPPLY AND ITS MANUFACTURING PROCESS | 2000 |
|
RU2187177C2 |
MANUFACTURING METHOD OF ACTIVE MASS OF CATHODE OF LITHIUM BATTERY | 2010 |
|
RU2424600C1 |
LITHIUM ACCUMULATOR ANODE ACTIVE MASS MANUFACTURING METHOD | 2017 |
|
RU2658305C1 |
CONDUCTING COMPOSITE CARBO-CONTAINING MATERIAL AND METHOD OF ITS FABRICATION | 2008 |
|
RU2398312C2 |
CARBON-CONTAINING CATHODE MATERIAL AND A METHOD OF PRODUCING CATHODE FOR LITHIUM CHEMICAL CURRENT SOURCE | 1994 |
|
RU2095310C1 |
POSITIVE ELECTRODE AND PRIMARY LITHIUM CHEMICAL CURRENT SOURCE CONTAINING IT | 2021 |
|
RU2780802C1 |
METHOD OF PRODUCTION OF LITHIUM ACCUMULATOR CATHODE ACTIVE MASS | 2005 |
|
RU2329570C2 |
Authors
Dates
2023-08-01—Published
2023-03-14—Filed