FIELD: polymer chemistry. SUBSTANCE: water-emulsion polymerization of 50% of butyl acrylate total amount is accomplished in the presence of sodium dodecylbenzosulfonate and potassium persulfate at 90-95 C for 1 hr. Then a mix of butylacrylate, methacrylic acid, and pyrazolone-5 derivative at a 1.0: 0.2: 1.0-1.4 mass ratio is added to polymerization medium and another polymerization process is initiated. EFFECT: no coagulum produced after 6 months of storage. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING OF POLYMERS FOR CHEMICAL-PHOTOGRAPHY INDUSTRY | 1987 |
|
SU1464440A1 |
METHOD OF LATEX PREPARING FOR CHEMICAL-PHOTOGRAPHY INDUSTRY | 1990 |
|
SU1804076A1 |
METHOD FOR PREPARING ACRYLIC COPOLYMER AQUEOUS DISPERSION FOR PRESSURE-SENSITIVE GLUES | 2006 |
|
RU2315062C1 |
METHOD FOR PRODUCTION OF AQUEOUS DISPERSIONS OF (CO)POLYMERS | 1995 |
|
RU2076109C1 |
METHOD OF PREPARING LATEX WITH HOLLOW POLYMER PARTICLES | 1998 |
|
RU2128670C1 |
METHOD OF PREPARING WATER DISPERSIONS OF (CO)POLYMERS | 2002 |
|
RU2223280C1 |
NITRILE BUTADIENE LATEX, DIP LATEX COMPOSITION, DIP PRODUCT | 2021 |
|
RU2771752C1 |
PROCESS FOR PREPARING AQUEOUS DISPERSIONS | 0 |
|
SU1035033A1 |
BUTADIENE-NITRILE LATEX, LATEX COMPOSITION FOR IMMERSION DIPPING, DIPPED PRODUCT | 2021 |
|
RU2776174C1 |
METHOD OF OBTAINING LATEX | 2017 |
|
RU2676609C1 |
Authors
Dates
1994-04-15—Published
1990-07-10—Filed