FIELD: chemical technology. SUBSTANCE: salt solution is prepared at mole ratio of titanium and alkaline-earth element 1:1.5-1:2, at total element concentration 15-30 g/kg. Solution is applied at temperature 110-130 C, thermolysis is started at 120-140 C and performed with temperature increase at the rate 5-20 C/min up to temperature 700 C, not less. EFFECT: improved method of film coating preparing. 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING POLYIMIDE DIELECTRIC LAYER | 1992 |
|
RU2019548C1 |
METHOD OF PREPARING OF POLYIMIDE ANTIADHESION COATING | 1992 |
|
RU2021296C1 |
COMPOSITION FOR POSITIVE PHOTORESIST REMOVAL | 1989 |
|
SU1653442A1 |
COMPOSITION FOR POSITIVE PHOTORESIST REMOVAL | 1990 |
|
SU1734487A1 |
FLUOROPLASTIC SUBSTRATE METALLIZATION DEPOSITION METHOD | 1991 |
|
RU2020777C1 |
METHOD OF PRODUCING "SOL-GEL" COMPLEX FROM AT LEAST THREE METAL SALTS AND USE OF METHOD FOR PRODUCTION OF CERAMIC MEMBRANE | 2012 |
|
RU2608383C2 |
METHOD FOR RECEIVING COAT ON PRODUCT MADE OF NICKEL OR NICKEL-CONTAINING ALLOY AND COAT, RECEIVED BY THIS METHOD | 2006 |
|
RU2339736C2 |
ELECTROLYTE FOR DEPOSITION OF COATINGS ONTO VALVE METALS | 1992 |
|
RU2046156C1 |
METHOD OF PREPARING HIGH-TEMPERATURE SUPERCONDUCTING COATING | 1994 |
|
RU2081937C1 |
METHOD FOR PRODUCTION OF THIN FILMS BASED ON INDIUM-TIN OXIDE BY MICRO-PLOTTER PRINTING | 2022 |
|
RU2785983C1 |
Authors
Dates
1995-05-10—Published
1990-11-22—Filed