FIELD: foundry. SUBSTANCE: method for zirconium introduction into magnesium includes treatment of magnesium melt with magnesium-zirconium alloying composition. The latter is preliminarily heated up to 720-750 C and exposed to d.c. solenoid magnetic field at intensity of 2·105-5·105A/m along solenoid axis at speed of 2.0-5 m/s in cylindrical channel of nonmagnetic material. Temperature of magnesium melt is maintained within 730-780 C. EFFECT: higher efficiency. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF TREATMENT OF ALLOYING COMPOSITION MAGNESIUM- ZIRCONIUM AND GEAR FOR ITS REALIZATION | 2000 |
|
RU2196844C2 |
METHOD OF PRODUCING MAGNESIUM-ALUMINUM-ZINC-MANGANESE ALLOY COMPOSITIONS | 1989 |
|
RU1727403C |
METHOD OF PRODUCING PIG MASTER ALLOY MAGNESIUM-NEODYMIUM-ZIRCONIUM | 1989 |
|
SU1678075A1 |
METHOD FOR OBTAINING MAGNESIUM-NEODYMIUM-ZIRCONIUM PIG ALLOY | 1990 |
|
SU1737917A1 |
METHOD OF PRODUCTION OF MAGNESIUM-ZIRCONIUM-RARE-EARTH METAL ALLOYS | 2002 |
|
RU2234552C2 |
METHOD OF INOCULATION AND CASTING OF ALLOYS OF NON-FERROUS METALS AND A DEVICE FOR ITS REALIZATION | 2002 |
|
RU2230823C2 |
METHOD OF SEPARATION OF METAL-OXIDE-SALT MELTS AND DEVICE FOR REALIZATION OF THIS METHOD | 1999 |
|
RU2172354C2 |
PROCESS FOR MODIFYING MAGNESIUM-ALUMINIUM ALLOYS | 1986 |
|
SU1431346A1 |
MAGNESIUM-BASED ALLOY AND A METHOD FOR PREPARATION THEREOF | 2001 |
|
RU2215056C2 |
0 |
|
SU400629A1 |
Authors
Dates
1995-04-30—Published
1991-04-03—Filed