FIELD: processing of infusible rare metal ores. SUBSTANCE: before reduction tungsten concentrate is calcined within 2-4 h at 600-950 C. Smelting is carried out in the presence of aluminium, its quantity being 0.3-0.6 parts per 1 part of tungsten. EFFECT: improves efficiency of the method. 4 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING ELECTRODES OF TUNGSTEN BEARING MINERALS AND DEVICE TO IMPLEMENT THE SAME | 1993 |
|
RU2043862C1 |
METHOD OF PROCESSING TUNGSTEN-CONTAINING CONCENTRATES TO PREPARE TUNGSTIC ACID | 2000 |
|
RU2173300C1 |
METHOD OF MANUFACTURING COMPOSITE MATERIAL FROM TUNGSTEN-CONTAINING MINERAL RAW MATERIAL | 1995 |
|
RU2098232C1 |
METHOD OF SELECTIVE EXTRACTION OF MOLYBDENUM AND BISMUTH | 2000 |
|
RU2172790C1 |
METHOD OF PROCESSING SCHEELITE INDUSTRIAL PRODUCTS | 0 |
|
SU1770424A1 |
METHOD FOR PRODUCTION OF METALS AND ALLOYS | 1996 |
|
RU2095440C1 |
METHOD OF MANUFACTURING COMPOSITE MATERIAL FROM TUNGSTEN-CONTAINING MINERAL RAW MATERIAL BASED ON SCHEELITE CONCENTRATE | 1995 |
|
RU2098233C1 |
ALLOY FOR PERMANENT MAGNETS BASED ON IRON | 1993 |
|
RU2048691C1 |
METHOD OF CONTINUOUS PROCESSING OF MIXED COPPER-CONTAINING RAW MATERIAL | 1995 |
|
RU2081195C1 |
METHOD OF PYROMETALLURGICAL PROCESSING OF WASTES, DEPLETED MATERIALS AND USED UP ARTICLES | 2000 |
|
RU2172787C1 |
Authors
Dates
1994-01-30—Published
1992-05-14—Filed