FIELD: mechanical engineering. SUBSTANCE: mechanically activated mixture of serpentinite with a binder is preliminary interposed between friction surfaces. Dispersivity of the serpentinite is equal to 0.001-1 micron and 2-40 mass % of the serpentinite is used to prepare the mixture. EFFECT: simplified method.
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING FILMS ON FRICTION SURFACES | 1992 |
|
RU2006707C1 |
| PROCEDURE FOR APPLICATION OF ANTIFRICTION COATING | 2009 |
|
RU2414545C1 |
| NANOTECHNOLOGY-BASED ANTIFRICTION POWDERED COMPOSITION (VERSIONS), NANOTECHNOLOGY-BASED LUBRICANT COMPOSITION AND NANOTECHNOLOGY-BASED LUBRICATION METHOD | 2009 |
|
RU2415176C2 |
| RAIL HEAD AND WHEELSET TYRE FLANGE WEAR PROTECTION METHOD | 1994 |
|
RU2111141C1 |
| COMPOSITION FOR MODIFYING METALS AND RESTORING METALLIC SURFACES | 2000 |
|
RU2169208C1 |
| METHOD OF FABRICATING "CAPROLONE" PRODUCTS | 1994 |
|
RU2090363C1 |
| METHOD FOR PRODUCING OF SUBSTANCE FOR PROTECTIVE COATING AND METHOD FOR CREATING OF PROTECTIVE COATING ON SURFACE | 2005 |
|
RU2286400C1 |
| FRICTION MODIFIER | 2009 |
|
RU2420562C1 |
| COMPOSITION FOR TREATMENT OF FRICTION PAIRS AND METHOD OF ITS PRODUCING | 2000 |
|
RU2168662C1 |
| TRIBOTECHNICAL COMPOSITION | 2001 |
|
RU2188227C1 |
Authors
Dates
1994-01-30—Published
1992-12-22—Filed