FIELD: metallurgy. SUBSTANCE: after oxidizing, the method involves taking a metal sample for determining nitrogen content then, after pouring out of metal and before blowing with argon, 0.3 kg/t of aluminium and titanium in the amount [Ti,%]=[N,%] is introduced on the ladle bottom. After blowing, a sample of metal is taken for analyzing the aluminium content and steel is alloyed with aluminium to a content of 0.015-0.030%. In the process of annealing the steel of terminal thickness to the temperatures of secondary recrystallization steel is saturated with nitrogen for forming the particles of inhibitor phase AlN. EFFECT: higher efficiency.
Title | Year | Author | Number |
---|---|---|---|
SILICON ELECTRIC STEEL AND METHOD OF TREATMENT THEREOF | 1996 |
|
RU2096516C1 |
PROCESS OF PRODUCTION OF ANISOTROPIC ELECTRICAL SHEET STEEL | 1996 |
|
RU2098493C1 |
METHOD FOR PRODUCTION OF THIN-SHEET ELECTRICAL STEEL | 1990 |
|
RU2068448C1 |
ELECTROTECHNICAL ANISOTROPIC STEEL PRODUCTION METHOD | 1993 |
|
RU2048544C1 |
METHOD FOR PRODUCING ANISOTROPIC ELECTRICAL STEEL | 1994 |
|
RU2082771C1 |
METHOD OF PRODUCTION OF SHEET ELECTROTECHNICAL ANISOTROPIC STEEL | 2003 |
|
RU2233892C1 |
METHOD OF PRODUCING ANISOTROPIC ELECTRICAL STEEL | 1996 |
|
RU2095433C1 |
METHOD FOR PRODUCING ELECTRICAL STEEL WITH HIGH MAGNETIC DENSITY | 2002 |
|
RU2216601C1 |
METHOD FOR MANUFACTURE OF ANISOTROPIC ELECTRIC SHEET STEEL | 2002 |
|
RU2224030C2 |
METHOD OF PRODUCING ANISOTROPIC ELECTRICAL-SHEET STEEL | 1999 |
|
RU2150518C1 |
Authors
Dates
1994-12-15—Published
1990-08-07—Filed