FIELD: applying of hardening coating. SUBSTANCE: eroded surface of details is affected by mechanical treatment followed by degreasing which is carried out with the help of benzine or acetone. Then shot-blasting treatment and detonation spraying take places. The latter process is carried out in series (each comprises 10-20 shots) at interval 0.5-3.0 min, uninterrupted blowing of sublayer with compressed air at pressure 2-4 atm takes place. EFFECT: higher efficiency of the method. 3 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR APPLICATION OF HARDENING COATING TO METAL OR METAL-CONTAINING SURFACES | 1995 |
|
RU2105826C1 |
METHOD OF RESTORATION OF SECTORS OF NOZZLE SET SPLIT RING | 1994 |
|
RU2069137C1 |
METHOD OF PRODUCING COMPOSITE POWDER OF ALUMINUM-ZINC SYSTEM FOR COATING BY COLD GAS-DYNAMIC SPUTTERING | 2023 |
|
RU2820258C1 |
METHOD FOR RESTORING THE CRANK PIN OF THE CRANKSHAFT OF AN INTERNAL COMBUSTION ENGINE | 2021 |
|
RU2760138C1 |
METHOD OF THERMAL DIFFUSION ZINC COATING OF ARTICLES MADE OF HIGH-STRENGTH ALUMINUM ALLOYS | 2017 |
|
RU2644092C1 |
RESTORATION METHOD OF WORN-OUT SURFACES OF STEEL PARTS | 2013 |
|
RU2532738C1 |
METHOD FOR RESTORING SKIRTS OF PISTONS OF INTERNAL COMBUSTION ENGINES | 2003 |
|
RU2227088C1 |
CHROMATE-FREE CERAMIC COATING COMPOSITIONS | 2013 |
|
RU2673685C2 |
METHOD FOR APPLYING HYDROXYAPATITE COATING ON TITANIUM ALLOY IMPLANTS | 2022 |
|
RU2782100C1 |
METHOD OF RECONDITIONING CORRODED PART FROM SUPERALLOY OR HIGH-TEMPERATURE STEEL, CORRODED PART AND RECONDITIONED PART FROM SUPERALLOY OR HIGH-TEMPERATURE STEEL, METHOD OF MAKING RECONDITIONED PART FROM SUPERALLOY OR HIGH-TEMPERATURE STEEL | 1994 |
|
RU2107749C1 |
Authors
Dates
1997-08-20—Published
1995-07-13—Filed