FIELD: ferrous metallurgy. SUBSTANCE: method includes emptying blast furnace below cast iron notch axis, drying and cooling dried lining, calculation and loading first-blow charge. According to invention, before drying, on surface of lining along hearth perimeter, titanium-containing materials are placed, their amount being found from the relationship: C = (10-20) x F where C is titanium usage, kg, and F hearth cross- section area, sq.m. EFFECT: increased service life of hearth lining caused by deposition of titanium carbide and nitride on it.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FORMING PROTECTIVE SKULL IN BLAST FURNACE | 2003 |
|
RU2223331C1 |
METHOD FOR BLOWING-IN BLAST FURNACE | 1998 |
|
RU2132390C1 |
METHOD FOR START BLOWING OF BLAST FURNACE | 2002 |
|
RU2216597C1 |
METHOD FOR CREATING PROTECTION LINING SLAG ON LINING OF HEARTH AND WELL OF BLAST FURNACE | 2005 |
|
RU2291199C1 |
METHOD OF BLOWING-IN BLAST FURNACE | 1999 |
|
RU2163641C1 |
METHOD OF FORMING PROTECTIVE SLAG LINING IN BLAST FURNACE | 2004 |
|
RU2255114C1 |
METHOD OF FORMING PROTECTIVE SKULL IN BLAST FURNACE HEARTH | 2003 |
|
RU2223330C1 |
METHOD OF FORMING PROTECTIVE SKULL ON BLAST FURNACE HEARTH LINING | 2003 |
|
RU2223328C1 |
METHOD FOR BLOWING-IN OF BLAST FURNACE | 2002 |
|
RU2235788C2 |
METHOD OF BLAST-FURNACE BLOWING-IN | 1999 |
|
RU2164242C2 |
Authors
Dates
1997-09-20—Published
1995-08-02—Filed