FIELD: metallurgy. SUBSTANCE: process may be used for arc deposition of bottom drum of bath for hot alumozinc plating of steel strips. Damaged upper layer of barrel is removed by turning down on lathe. Ring collar having width equal to 0.01-0.03 length of barrel is built up on each edge of it. Arc deposition is performed along helical line from center of barrel to its edges. Arc deposition can be performed in opposite direction. EFFECT: increased resistance of drum and diminished welding deformations. 1 cl
Title | Year | Author | Number |
---|---|---|---|
ROLL | 1996 |
|
RU2095190C1 |
METHOD OF RECONDITIONING OF ROLLER | 1996 |
|
RU2089628C1 |
CAST IRON ROLL JOURNALS RESTORING METHOD | 2005 |
|
RU2283709C2 |
METHOD FOR RESTORING ROLLING ROLLS | 1998 |
|
RU2139156C1 |
METHOD FOR RESTORING CAST IRON ROLLING ROLLS WITH DAMAGED JOURNALS | 2004 |
|
RU2281846C1 |
METHOD FOR RESTORING ROLLING ROLLS | 2003 |
|
RU2245771C2 |
METHOD FOR REPAIRING ROLLING ROLL | 1998 |
|
RU2139764C1 |
METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL | 2002 |
|
RU2228958C2 |
METHOD FOR RESTORING ROLLING ROLLS | 2001 |
|
RU2202422C2 |
METHOD FOR RESTORING BANDED ROLLER | 2003 |
|
RU2242347C1 |
Authors
Dates
1998-06-20—Published
1997-04-11—Filed