FIELD: metallurgy, more specifically, steel melting in converters. SUBSTANCE: method includes application of coating to internal surface of slag pans. Coating is applied with the help of mixture of aqueous solution of aluminosilicate mortar in ratio of components within 1:(0.5-1.0) and orthophosphoric acid in the amount of 0.3-0.6% of mortar solution volume. Consumption of mortar is within the range of 3-6.5 kg/cu.m of slag pan. Pan internal surface is subjected to 2-5 cyclic heatings and subsequent cooling for 5-10 min in each cycle of heating and cooling. EFFECT: higher stability of slag pans. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF APPLYING PROTECTIVE COATING ON CONVERTER LINING | 1995 |
|
RU2094474C1 |
METHOD OF LIME PREPARATION FOR STEEL MELTING IN CONVERTER | 1997 |
|
RU2127767C1 |
METHOD FOR REPAIRING CONVERTER LINING | 1997 |
|
RU2132392C1 |
METHOD FOR PREPARING POURING LADLE IN THE PROCESS OF CONTINUOUS STEEL CASTING | 1994 |
|
RU2025202C1 |
METHOD FOR APPLICATION OF LINING SLAG TO CONVERTER LINING | 1997 |
|
RU2109072C1 |
METHOD FOR REPAIR OF CONVERTER LINING | 1997 |
|
RU2114919C1 |
METHOD OF PLACING LINEN OF CONVERTER | 1996 |
|
RU2101362C1 |
METHOD OF STEEL MELTING IN CONVERTER | 1997 |
|
RU2109071C1 |
METHOD FOR PROTECTING LADLE CAR FROM GROWING OVER AT MELTING IRONS WITH INCREASED CONTENT OF TITANOMAGNETITES | 2000 |
|
RU2179908C1 |
ELECTRIC FURNACE FOR SMELTING OF SYNTHETIC SLAG | 1995 |
|
RU2096490C1 |
Authors
Dates
1998-07-20—Published
1997-09-15—Filed