FIELD: foundry, production of bimetal pig iron billets. SUBSTANCE: invention is related specifically to manufacture of rolls by centrifugal method with use of flux. Flux includes nonmetal and metal components. Metal component has, per cent by mass: silicon oxide 20.0-25.0; calcium oxide 25.0- 35.0; calcium fluoride 20.0-25.0; sodium fluoride 2.0-3.0; borax 10.0-15.0; aluminum oxide up to 1.5; magnesium oxide up to 1.5; potassium chloride ( sodium chloride ) 5.0-10.0. Nonmetal component includes aluminum powder up to 0.5 and ferroalloy powder 1.0-3.0 per cent by mass. Injection of aluminum powder into nonmetal component results in increased refining properties of flux and ferroalloy powder provides for modification of pig iron. EFFECT: increased refining properties of flux and modification of pig iron.
Title | Year | Author | Number |
---|---|---|---|
FLUX FOR CENTRIFUGAL CASTING | 2004 |
|
RU2262413C1 |
FLUX FOR CENTRIFUGAL CASTING OF BIMETAL BLANKS | 2007 |
|
RU2353467C1 |
METHOD OF CENTRIFUGAL CASTING OF BIMETAL CAST IRON BLANKS | 1998 |
|
RU2117548C1 |
CAST IRON | 1998 |
|
RU2124066C1 |
FLUX FOR MECHANIZED WELDING AND SURFACING OF STEELS | 2020 |
|
RU2749735C1 |
FLUX FOR SPUN CASTING | 2011 |
|
RU2479378C1 |
FLUX FOR CENTRIFUGAL CASTING OF TWO-LAYER IRON ROLLING ROLLS | 0 |
|
SU961853A1 |
FLUX FOR STEEL MECHANISED WELDING AND SURFACING | 2014 |
|
RU2579412C2 |
METHOD OF CENTRIFUGAL CASTING OF ROLLS | 1996 |
|
RU2109595C1 |
COMBINED FLUX FOR SMELTING BRASSES | 1995 |
|
RU2081928C1 |
Authors
Dates
1998-12-10—Published
1998-02-27—Filed