FIELD: chemical technology. SUBSTANCE: anode surface around replaceable pins is slightly dried 12-24 hours prior to installation of pins by adding additional amount of correcting anode compound having reduced amount of binder. In order to preserve shape of hole for pin, plug made of nonferromagnetic material with diameter equal to that of pin is inserted into hole. EFFECT: reduced consumption of anode compound and improved labor conditions. 2 cl, 2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
SELF-FIRED ANODE MAKING METHOD | 2005 |
|
RU2307879C2 |
ALUMINUM CELL SELF-FIRED ANODE FORMING METHOD | 2005 |
|
RU2308548C2 |
METHOD OF FORMING SECONDARY ANODE OF ALUMINIUM ELECTROLYSER WITH SODERBERG TYPE ANODE AND UPPER CURRENT SUPPLY | 2013 |
|
RU2536321C1 |
METHOD OF FORMING A SECONDARY ANODE OF AN ALUMINUM ELECTROLYSIS CELL WITH A SELF-BAKING ANODE | 2019 |
|
RU2698121C1 |
PIN FOR APPLYING ELECTRIC CURRENT TO SELF-FIRED ANODE OF ALUMINUM CELL | 2006 |
|
RU2318923C1 |
METHOD FOR FORMING OF SECONDARY ANODE FOR ALUMINUM ELECTROLYZER WITH SELF-ROASTING ANODE AND UPPER CURRENT SUPPLY (VERSIONS) | 2005 |
|
RU2286403C1 |
METHOD OF REARRANGEMENT OF THE ANODE RODS IN THE ELECTROLYZER, WHICH HAS THE SELF-CALCINING ANODE AND THE UPPER FEEDING OF THE ELECTRIC CURRENT | 2006 |
|
RU2312937C1 |
METHOD OF MAINTAINING SELF-BURNING ANODE IN ELECTROLYZERS WITH UPPER POWER SUPPLY | 1994 |
|
RU2092621C1 |
METHOD OF FORMING SELF-FIRING ANODE FOR ALUMINIUM ELECTROLYZER | 0 |
|
SU1608251A1 |
PROCEDURE FOR FORMING SELF-CALCINATING COAL ANODE OF ALUMINIUM ELECTROLYTIC CELL | 2009 |
|
RU2397277C1 |
Authors
Dates
2000-04-27—Published
1998-10-30—Filed