FIELD: ferrous metallurgy; method of hot repair of converter lining. SUBSTANCE: in applying the slag lining, slag-forming materials containing Ca and Mg are introduced in succession on slag remaining in converter after previous heat at two stages. At first stage, Ca-containing materials are added and slag melt thus obtained is mixed by mixture of neutral gas with oxygen at ratio of 1(0.05-0.15). At second stage, Mg- containing materials in the amount of 20 to 50% of mass of Ca-containing materials added at first stage are added and Mg-containing materials are mixed with slag melt by neutral gas. Ratio of mixing time at first stage to mixing time at second stage is maintained within 1:(1.3-1.5). Then, slag melt is applied on lining by jets of neutral gas. EFFECT: enhanced efficiency and stability. 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
COVERING METHOD OF SLAG-SKIN ON VESSEL LINING | 2006 |
|
RU2342444C2 |
METHOD OF STEEL MELTING IN CONVERTER | 2000 |
|
RU2177508C1 |
METHOD OF REPAIR OF CONVERTER LINING AND LANCE FOR REALIZATION OF THIS METHOD | 2004 |
|
RU2273669C1 |
METHOD OF LINING OF OXYGEN STEEL-MAKING CONVERTER | 2000 |
|
RU2164953C1 |
METHOD OF SKULL APPLICATION TO CONVERTER LINING | 1997 |
|
RU2128714C1 |
METHOD OF DEPOSITION OF THE WALL ACCRETION ON THE CONVERTER BRICK-LINING | 2005 |
|
RU2294379C1 |
METHOD OF PROTECTIVE SCULL FORMING ON OXYGEN CONVERTER LINING SURFACE AND MAGNESIAN BRIQUETTED FLUX (MBF) FOR ITS IMPLEMENTATION | 2015 |
|
RU2606351C2 |
PROCEDURE FOR APPLICATION OF SLAG SCULL ON CONVERTER LINING | 2008 |
|
RU2397253C1 |
METHOD OF APPLYING WALL ACCRETION TO CONVERTER LINING | 2008 |
|
RU2373291C1 |
METHOD OF APPLYING SLAG SKULL ON REFRACTORY LINING OF OXYGEN CONVERTER | 2024 |
|
RU2826359C1 |
Authors
Dates
2001-07-10—Published
1999-08-09—Filed