FIELD: rolled stock production, possibly method of operation of steel rolling rolls of cold rolling mills. SUBSTANCE: method comprises steps of low-temperature tempering of roll before starting its operation; soaking it at temperature 160 - 190 C during time period equal to (0.1 - 0.3)HSD hours; operation of roll in stand and forced idling of it including heating stage at rate 25 - 80 C/h , soaking stage at 170 - 250 C during 6 - 20 h and cooling stage at rate 10 -60 C/h; realizing idling after roll operation period providing rolling of 45 - 50% of normalized rolled metal quantity at preliminarily removing by working surface layer of roll with thickness equal to (0.001 -0.01)HSD mm, where HSD - hardness of roll barrel according to Shore. EFFECT: reduced number of crumblings and scalings of hardened layer of roll. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ROLLING ROLLER EXPLOITATION | 1992 |
|
RU2015757C1 |
ROLLING ROLL OPERATION METHOD | 1999 |
|
RU2164181C2 |
METHOD FOR OPERATION OF ROLL | 1997 |
|
RU2107566C1 |
METHOD OF ROLL OPERATION | 1997 |
|
RU2104811C1 |
METHOD FOR RESTORING ROLLING ROLLS | 1998 |
|
RU2139156C1 |
METHOD OF BUILDING UP ROLLS | 2002 |
|
RU2218220C1 |
METHOD OF OPERATION OF SHEET ROLLING ROLL | 1998 |
|
RU2126730C1 |
ROLLING ROLL OPERATION METHOD | 2003 |
|
RU2240879C1 |
ROLLING ROLL OPERATION METHOD | 1999 |
|
RU2147944C1 |
BACKUP ROLL OPERATION METHOD | 2004 |
|
RU2278751C1 |
Authors
Dates
2003-01-27—Published
2001-05-30—Filed