FIELD: machine engineering, possibly manual and automatic electric arc welding of high- strength heat resistant and refractory steels in inert gas atmosphere. SUBSTANCE: activating flux includes (mass %): lithium hexafluoroaluminate, 20 - 30; titanium dioxide, 20 - 30; alumina, 10 - 30; calcium chloride 20 - 30. EFFECT: enhanced welding-through capability of welding arc, stable formation of welded seam. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ACTIVATING FLUX FOR ELECTRIC ARC WELDING | 2005 |
|
RU2291039C1 |
ACTIVATING FLUX FOR ELECTRIC ARC WELDING | 2000 |
|
RU2164849C1 |
ACTIVATING FLUX FOR ARC WELDING | 2005 |
|
RU2289498C1 |
METHOD OF ELECTRIC ARC WELDING WITH USE OF ACTIVATING FLUX | 2002 |
|
RU2224630C1 |
ELECTRIC ARC WELDING METHOD | 2001 |
|
RU2188105C1 |
ELECTRIC ARC WELDING METHOD | 2001 |
|
RU2187415C1 |
ACTIVATING FLUX FOR ELECTRIC ARC WELDING OF STAINLESS AND HIGH-STRENGTH STEELS | 0 |
|
SU1342649A1 |
ELECTRIC ARC WELDING METHOD | 2001 |
|
RU2209714C2 |
ELECTRIC ARC WELDING METHOD WITH USE OF ACTIVATING MATERIAL | 2004 |
|
RU2264897C1 |
NANOSTRUCTURED WELDING MATERIAL | 2013 |
|
RU2544317C2 |
Authors
Dates
2003-02-20—Published
2001-04-16—Filed