FIELD: production of strip and making electrical sheet steel with grain oriented in planes (110)[001].
SUBSTANCE: continuously cast thin strip is subjected to hot rolling and annealing for re-crystallization of structure. Parameters of technological process are so selected that strain/re-crystallization index (K*)-1≥ is about 6500. This index is found from the following formula: (K*)-1= (THBA)1n[ε-0.15exp(7616THR)1n(tc/tf)], where THBA is strip annealing temperature, K; ε is intensity of strain at hot rolling; tc is initial thickness of strip before hot rolling and tf is final thickness of strip after hot rolling.
EFFECT: enhanced efficiency and reliability.
3 dwg, 4 tbl, 2 ex