FIELD: medicine.
SUBSTANCE: method involves placing bone implant in 2-5% tripsin solution at temperature 30-40°С for 6-8 h. Then, bone implant washing is carried out in turn with physiological solution and 2-5% tripsin solution at the same temperature. Alternation frequency rate depends on morphologically determined final bone implant cleaning degree. Final washing is carried out with physiological salt solution.
EFFECT: enhanced effectiveness of treatment; improved plastic bone implant properties, full bone marrow removal; accelerated implant preparation to clinical use or morphological research.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING BONE IMPLANTS | 2013 |
|
RU2526429C1 |
METHOD FOR MANUFACTURING OSSEOUS IMPLANTS | 2004 |
|
RU2268060C1 |
METHOD OF OBTAINING BONE IMPLANT ON THE BASIS OF STERILE DEMINERALIZED BONE MATRIX | 2018 |
|
RU2679121C1 |
METHOD OF BONE CLEANING | 2010 |
|
RU2438308C1 |
METHOD FOR BONE SAMPLES MACHINING IN VITRO | 2016 |
|
RU2629664C1 |
METHOD FOR MAKING LARGE-BLOCK FREEZE-DRIED BONE IMPLANTS | 2008 |
|
RU2366173C1 |
METHOD FOR REMOVING BONE MARROW OF ALLOTRANSPLANT | 1992 |
|
RU2033795C1 |
METHOD OF PRODUCING ALLOGENIC BONE-REPLACEMENT MATERIAL | 2019 |
|
RU2715238C1 |
METHOD FOR OBTAINING OSSEOUS TRANSPLANT | 2001 |
|
RU2223104C2 |
METHOD OF MANUFACTURING SPONGY BONE TRANSPLANTS | 2010 |
|
RU2440730C1 |
Authors
Dates
2007-06-27—Published
2005-12-27—Filed