FIELD: chemistry.
SUBSTANCE: anticorrosion mastic is obtained in a single process cycle. The process involves loading bitumen at 130°C. Technical sulphuric acid is then added for 1.5-2 hours at 130°C. Further, the product is stabilised at 150°C for 4 hours. Additives are then added - industrial oil, butyl rubber, thermoplastic elastomer - at 140°C. The components are continuously stirred after each process cycle for 60-180 minutes.
EFFECT: improved physical and chemical characteristics of the obtained anticorrosion mastic owing to improvement of its composition and optimisation of the production technology.
3 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ANTI-CORROSION MASTIC MATERIAL | 2008 |
|
RU2384601C2 |
COILED MASTIC MATERIAL | 2008 |
|
RU2379575C2 |
ROLLED MASTIC MATERIAL ON TEXTILE BASE TAPE IMPREGNATED WITH MASTIC USING ASPHALTIC RESINOUS OLIGOMERS (VERSIONS) | 2010 |
|
RU2458282C2 |
INSULATION COMPOSITION AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2508304C1 |
ASMOL PRODUCTION METHOD AND ANTICORROSIVE INSULATING TAPE | 2020 |
|
RU2746727C1 |
MASTIC COMPOSITION AND METHOD OF OBTAINING THEREOF | 2013 |
|
RU2543217C1 |
METHOD OF PRODUCING INSULATION COMPOSITION (VERSIONS) | 2017 |
|
RU2656486C1 |
MASTIC | 2008 |
|
RU2368637C1 |
POLYMER-BITUMEN BINDER | 2013 |
|
RU2562496C2 |
METHOD OF PRODUCING ANTICORROSION MATERIAL | 1994 |
|
RU2074224C1 |
Authors
Dates
2010-12-27—Published
2009-02-12—Filed