FIELD: machine building.
SUBSTANCE: method includes saturation of a cutting edge with strengthening elements from a plaster containing 84 or 90 wt % of boron carbide and 16 or 10 wt % of a fused flux for induction fusing P-0.66. The plaster is applied onto the cutting edge and the actuator's tip at the side contacting with soil, saturation is carried out with high-frequency currents with heating of the saturated surface up to the temperature of 1250-1300°C and soaking time of 1-2 min. Subsequent thermal treatment is carried out by heating of the entire tiller up to 850-900°C with subsequent tempering in the oil medium. The fused flux for induction fusing P-0.66 contains modifiers, such as a mixture of a silicocalcium powder 20 wt % and a powder of flux AN-348A 80 wt %.
EFFECT: increased thickness of a wear resistant layer, higher ecological compatibility of the process and reduced time of the technological process.
2 cl, 3 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR INDUCTION SURFACING OF WEAR-RESISTANT ALLOY | 2020 |
|
RU2755913C1 |
METHOD FOR SURFACING IRON ALUMINIDE ON STEEL SURFACE | 2018 |
|
RU2693988C1 |
METHOD OF PRODUCING MOULDED STEEL PART | 2015 |
|
RU2622503C2 |
METHOD TO STRENGTHEN SURFACE OF CAST STEEL PART | 2016 |
|
RU2641209C1 |
METHOD OF STRENGTHENING BLADE SURFACE OF PART | 2016 |
|
RU2640515C1 |
METHOD FOR APPLICATION OF CERAMIC COATING ONTO PARTS FROM CAST IRON AND STEEL | 2011 |
|
RU2482215C1 |
BORON-ALUMINIZING METHOD OF STEEL SURFACE | 2018 |
|
RU2691431C1 |
METHOD FOR INDUCTION HARDENING OF TILLAGE WORKING BODY | 2014 |
|
RU2582840C1 |
METHOD OF HARDENING OF CULTIVATOR BLADE | 2018 |
|
RU2684127C1 |
METHOD OF MANUFACTURING OF TILLAGE LANCET-TYPE WORKING ELEMENT | 2011 |
|
RU2474098C1 |
Authors
Dates
2012-04-10—Published
2010-08-03—Filed