FIELD: metallurgy.
SUBSTANCE: molybdenum or tungsten compounds with a boron compound are reduced with metallic magnesium in a molten salt mixture medium of NaCl-NaF (1:1) at a temperature of 800-900°C. The ratio of oxides of molybdenum or tungsten compound with boron is maintained at 1:2.5 of mass fraction, and the ratio of molybdenum or tungsten oxides with magnesium is 1:0.45 of mass fraction.
EFFECT: production of composite fine powders of Mo-MoB, W-WB with a low content of impurities at low temperatures is provided.
2 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING A COMPOSITE MATERIAL WB-WC-AlO FROM A SCHEELITE CONCENTRATE OF THE FAR EAST REGION | 2020 |
|
RU2758654C1 |
METHOD FOR PRODUCING NANODISPERSED ISOTOPE-MODIFIED MOLYBDENUM BORIDE | 2023 |
|
RU2811828C1 |
ELECTROCHEMICAL METHOD TO PRODUCE MOLYBDENE BORIDE | 2015 |
|
RU2629188C2 |
METHOD FOR PRODUCING POWDERS OF MOLYBDENUM OR ITS COMPOSITES WITH TUNGSTEN | 2005 |
|
RU2285586C1 |
METHOD FOR PRODUCING MOLTEN CERMET COMPOSITE MATERIAL, MOLDED CERMET COMPOSITE MATERIAL PRODUCED BY THE METHOD, MOLDED COMPOSITION (VERSIONS) AND METHOD FOR PRODUCING METALLIC ALUMINUM | 1992 |
|
RU2114718C1 |
ALUMINUM-BOR LIGATURE ALLOY PRODUCTION METHOD | 2015 |
|
RU2610182C2 |
METHOD FOR PRODUCING ALUMINA-MATRIX COMPOSITE MATERIALS | 2021 |
|
RU2768800C1 |
METHOD FOR OBTAINING METALLIC TUNGSTEN POWDER | 2003 |
|
RU2243063C1 |
METHOD OF PRODUCING MAGNETIC-ABRASIVE POWDER | 2018 |
|
RU2697139C1 |
CERAMIC COMPOSITE AND BATCH FOR ITS PRODUCING | 2015 |
|
RU2622276C2 |
Authors
Dates
2012-07-10—Published
2010-06-24—Filed