FIELD: metallurgy.
SUBSTANCE: invention relates to manufacture of consumable electrode for melting ingots of titanium-aluminium alloys containing 15-63 wt % of aluminium. Method comprises preparing a charge by mixing titanium sponge and semi-finished aluminium product, charge portion flow into conical matrix and subsequent through-feed pressing. Titanium sponge is used in the form of spherical bodies with a diameter of 10-25 mm, and aluminium semi-finished product - in the form of bars with the diameter : length ratio = 1:1. Ratio of linear aluminium semi-finished product dimensions to linear titanium sponge dimensions is 2.5-3.5.
EFFECT: increased mechanical properties of electrodes.
2 cl, 6 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR MANUFACTURING TITANIUM ALLOY INGOTS | 1991 |
|
RU2031174C1 |
METHOD TO PRODUCE INGOT OF PSEUDO β-TITANIUM ALLOY, CONTAINING (4,0-6,0)%Al, (4,5-6,0)% Mo, (4,5-6,0)% V, (2,0-3,6)%Cr, (0,2-0,5)% Fe, (0,1-2,0)%Zr | 2010 |
|
RU2463365C2 |
CONSUMABLE ELECTRODE FOR VACUUM ARC FURNACE AND METHOD OF MAKING IT | 2008 |
|
RU2359432C1 |
CONSUMABLE ELECTRODE FOR PRODUCING HIGH TITANIUM FERRO ALLOY BY MEANS OF ELECTRO SLAG MELTING | 2005 |
|
RU2335553C2 |
SECONDARY TITANIUM ALLOY AND PROCEDURE FOR ITS FABRICATION | 2010 |
|
RU2425164C1 |
METHOD FOR SEMI-CONTINUOUS PRESSING OF ARTICLES OF TITANIUM ALLOY CHARGE MATERIALS | 2004 |
|
RU2264887C1 |
CONSUMABLE ELECTRODE FORMING METHOD | 2002 |
|
RU2234543C2 |
METHOD OF PRODUCING OF INTERMETALLIC ALLOYS BASED ON TITANIUM ALUMINIDE WITH INCREASED NIOBIUM CONTENT | 2014 |
|
RU2576288C1 |
METHOD OF MANUFACTURING AN ELECTRODE OF TITANIUM SPONGE, ALLOYING COMPONENTS, WASTES OF TITANIUM ALLOYS | 2016 |
|
RU2671521C2 |
METHOD OF SEMICONTINUOUS MOLDING OF ARTICLES FROM CHARGE MATERIALS OF TITANIUM ALLOYS | 1997 |
|
RU2120351C1 |
Authors
Dates
2017-03-21—Published
2015-10-21—Filed