FIELD: chemistry.
SUBSTANCE: method comprises granulating an aluminium powder consisting of plate-shaped particles with stearic coating, pressing the preform from the granular powder and sintering it. Granulation is carried out by heat treatment of the powder in air at the temperature of 375-380°C for 3-5 hours and its subsequent heat treatment in a vacuum at the temperature of 620-650°C for 1-2 hours, the pressing of the preform is carried out at the pressure of 500-1000 MPa, and sintering of the preform is carried out at the temperature of 570-600°C for 1-2 hours.
EFFECT: increasing the relative density and specific effective work of the composite material fracture.
2 cl, 3 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2015 |
|
RU2592917C1 |
METHOD FOR OBTAINING LAYERED CERMET Al-AlO-AlC | 2022 |
|
RU2783786C1 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2015 |
|
RU2583966C1 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2011 |
|
RU2461530C1 |
METHOD FOR OBTAINING POROUS ALUMINIUM OXIDE CERAMICS | 2015 |
|
RU2610482C1 |
METHOD OF PRODUCTION OF COMPOSITE MATERIAL AlO-Al | 2006 |
|
RU2319678C1 |
METHOD OF OBTAINING COMPOSITE MATERIAL Al-AlO | 2012 |
|
RU2521009C1 |
METHOD FOR PRODUCING ANTIFRICTION ALUMINIUM MATRIX COMPOSITE MATERIAL | 2022 |
|
RU2796870C1 |
METHOD FOR PRODUCING ALUMINIUM-TITANIUM COMPOSITE MATERIAL | 2023 |
|
RU2799643C1 |
METHOD OF OBTAINING A COMPOSITE MATERIAL AlO-Al | 2022 |
|
RU2799462C1 |
Authors
Dates
2017-10-04—Published
2016-03-15—Filed