FIELD: metallurgical engineering.
SUBSTANCE: at the pelletiser bottom there formed scull: charge is supplied to the pelletiser in two flows. The first flow of charge is introduced into the gas stream with formation of gas-moisture-charge jet into which pore-forming additives are fed. As pore-forming additives, phytogenic particles grounded to the needle state or vegetable waste from agricultural production are used. At the pelletiser bottom there formed is a zone occupied with charge and a zone free from charge. The charge is sprayed on the skull in a zone free of charge, with the formation of a dense layer of wet charge, which is divided into nuclei, precombusting the embryos to the pellets with a charge of the second stream, drying and roasting them. In this case, the pore-forming additives are preliminarily soaked in a sulfite-fat distiller's beer for 0.1-3.0 hours at a temperature of 30-90°C.
EFFECT: increase in strength and yield of conditioning pellets.
1 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING PELLETS | 2022 |
|
RU2782895C1 |
METHOD OF PRODUCING PELLETS | 2019 |
|
RU2698000C1 |
METHOD OF MAKING PELLETS | 2018 |
|
RU2679853C1 |
PROCEDURE FOR PRODUCTION OF PELLETS | 2010 |
|
RU2423533C1 |
PELLET PRODUCING METHOD | 2020 |
|
RU2743435C1 |
METHOD FOR PRODUCING PELLETS | 2022 |
|
RU2790521C1 |
METHOD OF PRODUCING PELLETS | 2019 |
|
RU2717749C1 |
PELLET OBTAINING METHOD | 2011 |
|
RU2464328C1 |
PELLET OBTAINING METHOD | 2013 |
|
RU2529140C1 |
PELLET OBTAINING METHOD | 2013 |
|
RU2537982C1 |
Authors
Dates
2017-10-31—Published
2016-12-28—Filed