FIELD: woodworking industry.
SUBSTANCE: group of inventions relates to wood modification. To obtain modified wood, wood is treated with wood resin having moisture content of at least 10 %, where the resin solution contains phenol-formaldehyde, urea-formaldehyde resin, melamine resin, lignin, tannin or a mixture thereof. Then, a thermal modification stage is carried out, where the wood is heated at temperature of 160 to 230 °C at atmospheric pressure or at temperature of 120 to 230 °C at pressure above atmospheric pressure.
EFFECT: higher hardness of surface and biological stability of wood material.
8 cl
Title | Year | Author | Number |
---|---|---|---|
MODIFIED WOOD PRODUCT AND METHOD FOR PRODUCING SAID PRODUCT | 2018 |
|
RU2765891C2 |
PRODUCT OF MODIFIED WOOD AND METHOD OF ITS PRODUCTION | 2017 |
|
RU2745502C2 |
COMPOSITE PRODUCT AND PROCESS FOR PRODUCTION THEREOF | 2016 |
|
RU2701536C2 |
METHOD FOR FORMING WOOD FIBRE | 2014 |
|
RU2716776C2 |
PROCESS FOR MANUFACTURING PRODUCTS FROM ACETYLATED WOOD FIBRE | 2014 |
|
RU2717224C2 |
COMPOSITE MATERIAL AND COMPOSITE PRODUCT | 2018 |
|
RU2757685C2 |
METHOD FOR MICROWAVE WOOD WORKING | 2002 |
|
RU2285875C2 |
COMPOSITE PRODUCT AND TECHNOLOGICAL PROCESS OF PRODUCTION OF SAID PRODUCT | 2016 |
|
RU2737697C2 |
ARTIFICIAL WOOD MATERIALS AND PRODUCTION METHODS | 2016 |
|
RU2724496C2 |
METHOD OF MANUFACTURING PRODUCT FROM DENSE WOOD | 2020 |
|
RU2811112C1 |
Authors
Dates
2020-04-17—Published
2016-09-28—Filed