FIELD: metallurgy.
SUBSTANCE: invention relates to production of articles from titanium alloys using additive technologies. Titanium alloy contains, wt %: aluminum 2.0–6.0, vanadium 4–8.75, iron 1.0–5.0, rest is titanium, unavoidable impurities and one or more optional secondary elements, selected from silicon to 1 wt %, yttrium to 1 wt %, erbium to 1 wt %, carbon to 0.5 wt %, oxygen to 0.5 wt % and boron to 0.5 wt %. Amount of titanium, aluminum, vanadium and iron in the alloy is sufficient to provide beta-transition temperature of not more than 850 °C. Article made of titanium alloy is produced by application of successive layers of raw material and then selective melting with formation of article.
EFFECT: obtaining material with a high liquidus point and a narrow equilibrium crystallisation interval which limits microsegregation during hardening.
20 cl, 4 dwg, 5 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PERFECTED ALUMINIUM-COPPER ALLOYS CONTAINING VANADIUM | 2010 |
|
RU2524288C2 |
IMPROVED FINISHING METHODS OF EXTRUDED TITANIUM ARTICLES | 2017 |
|
RU2709568C1 |
ALUMINIUM-LITHIUM ALLOYS OF 2XXX SERIES | 2012 |
|
RU2587009C2 |
2XXX SERIES ALUMINUM LITHIUM ALLOYS | 2013 |
|
RU2659529C2 |
IMPROVED DENSE FORGED ALLOYS BASED ON 7XXX ALUMINUM AND METHODS FOR THEIR PRODUCTION | 2018 |
|
RU2745433C1 |
IMPROVED THICK WROUGHT ALUMINIUM 7XXX ALLOYS AND METHODS FOR PRODUCTION THEREOF | 2016 |
|
RU2752487C2 |
ALLOYS BASED ON ALUMINIUM AND LITHIUM OF 2XXX SERIES | 2019 |
|
RU2815234C2 |
METHODS OF ARTICLES PRODUCTION BY MEANS OF ADDITIVE PRODUCTION | 2017 |
|
RU2705841C1 |
ALLOY Al-Zn-Mg-Cu | 2004 |
|
RU2353693C2 |
METHODS OF PRODUCING FORGED ARTICLES AND OTHER PROCESSED ARTICLES | 2017 |
|
RU2702888C1 |
Authors
Dates
2020-08-07—Published
2017-04-24—Filed