FIELD: metallurgy.
SUBSTANCE: asymmetric rolling is carried out with a reduction of 80-86% in one pass, while the circumferential speeds of the rolls are set based on the following ratio: V2/V1=4-5, where: V1 is the circumferential speed of the upper work roll, rpm; V2 is the circumferential speed of the lower work roll, rpm. Then symmetrical rolling of the strip is carried out with a total reduction of not more than 86%.
EFFECT: plasticity of the aluminium alloy strip and isotropy of mechanical properties over its entire cross-section are ensured.
1 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ASYMMETRIC ROLLING OF COLD-ROLLED STRIP FROM ALUMINIUM ALLOY “АД33” | 2023 |
|
RU2820860C1 |
METHOD FOR ASYMMETRIC ROLLING OF COLD-ROLLED STRIP MADE OF ALUMINIUM ALLOY AMg6 | 2022 |
|
RU2793650C1 |
METHOD FOR ASYMMETRIC ROLLING OF D6 ALUMINIUM ALLOY STRIP (EMBODIMENTS) | 2022 |
|
RU2794211C1 |
METHOD OF PRODUCTION OF STRIPS FROM HIGH-CARBON AND ALLOY STEELS | 2023 |
|
RU2795066C1 |
METHOD OF PRODUCING BELT FROM LOW-CARBON STEELS | 2023 |
|
RU2821127C1 |
METHOD OF OBTAINING SHEET FROM ALUMINUM-MAGNETIC ALLOYS | 2018 |
|
RU2677196C1 |
METHOD OF THIN-SHEET ROLLING ALUMINIUM ALLOYS | 2016 |
|
RU2622195C1 |
METHOD OF PRODUCING A THIN STRIP | 2019 |
|
RU2701322C1 |
ASYMMETRICAL CRYOGENIC ROLLING METHOD | 2019 |
|
RU2699432C1 |
COLD-ROLLED STRIP MANUFACTURING METHOD | 2013 |
|
RU2542212C1 |
Authors
Dates
2023-07-25—Published
2023-04-11—Filed