FIELD: electrical engineering and radio engineering.
SUBSTANCE: invention relates to the production of soft magnetic composite material (SMCM). The magnetically soft composite material comprises iron powder with a low oxygen content and additionally comprises a mixture of sodium and potassium salts. The ratio of the components is as follows, wt.%: mixture of salts 0.2-1.0, iron powder is the rest, and the mixture of salts comprises wt.%: NaCl 30-40%; KCl 30-40%; Na2CO3 20-40%.
EFFECT: creating a soft magnetic composite material from iron powder and environmentally friendly harmless components with high magnetic properties.
1 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING POWDERS OF MOLYBDENUM OR ITS COMPOSITES WITH TUNGSTEN | 2005 |
|
RU2285586C1 |
MAGNETICALLY-SOFT COMPOSITE MATERIALS | 2006 |
|
RU2389099C2 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2015 |
|
RU2592917C1 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2011 |
|
RU2461530C1 |
COMPOSITION OF POWDER, METHOD FOR MANUFACTURE OF SOFT MAGNETIC COMPONENTS AND SOFT MAGNETIC CONSTITUENT | 2004 |
|
RU2326461C2 |
SOFT MAGNETIC COMPOSITE MATERIAL | 2011 |
|
RU2469430C1 |
METHOD OF PRODUCTION OF COMPOSITE MATERIAL AlO-Al | 2006 |
|
RU2319678C1 |
NEW COMPOSITE MATERIAL AND METHOD OF ITS MANUFACTURE | 2012 |
|
RU2631246C2 |
METHOD OF PRODUCTION OF COMPOSITE MATERIAL AlO-Al | 2004 |
|
RU2266270C1 |
METHOD OF PRODUCING ALLOYED POWDERS IN VIBROFLUIDISED BED | 2015 |
|
RU2606358C2 |
Authors
Dates
2023-12-27—Published
2023-07-11—Filed