FIELD: measurement technology. SUBSTANCE: adhesive of 8 to 16 microns in thickness is applied to metallized film. The latter is exposed to 60 C for 6 minutes, 65 C for 8 minutes, and 70 C for 10 minutes. Then temperature is raised to 150-170 C and maintained for 15-20 minutes, film is cooled down and stack of films is formed. Stack is exposed to pressure of 2 or 3 MPa for 120 -160 minutes at 150 to 170 C. EFFECT: improved reliability and technological effectiveness of pressure transducers for aerodynamic tests of aircraft equipment. 1 dwg