FIELD: soldering materials. SUBSTANCE: metal-crystalline solder consisting of low-melting component and refractory component that contains nickel and titanium. Low-melting component has alloy aluminium-silicon-magnesium and refractory component has additionally bismuth at the following ratio of components, weight %: low-melting component 50-90, refractory component 10-50. Refractory component has the following components, weight %: bismuth 1-10; nickel 20-45, and titanium - the rest. EFFECT: improved quality of solder.
Title | Year | Author | Number |
---|---|---|---|
SOLDER FOR FLUXLESS SOLDERING | 1992 |
|
RU2012468C1 |
MIXED POWDER SOLDER FOR SOLDERING ALUMINUM AND ALLOYS BASED ON IT | 2021 |
|
RU2779439C1 |
METHOD FOR COMPOSITION SOLDERING OF ALUMINIUM AND ITS ALLOYS | 1997 |
|
RU2129060C1 |
SOLDER FOR SOLDERING ALUMINIUM AND ALLOYS THEREOF | 2014 |
|
RU2596535C2 |
SOLDER FOR SOLDERING ALUMINIUM AND ALLOYS THEREOF | 2014 |
|
RU2585598C1 |
MULTILAYER ALUMINIUM SHEET FOR FLUX-FREE HIGH TEMPERATURE BRAZING IN CONTROLLED ATMOSPHERE | 2013 |
|
RU2642245C2 |
METHOD OF MAKING ABRASIVE TOOL FROM SUPERHARD MATERIALS | 2010 |
|
RU2457935C2 |
METHOD FOR PRODUCTION OF ABRASIVE DIAMOND TOOL | 2007 |
|
RU2362666C1 |
COMPOSITE SOLDER FOR SOLDERING ABRASIVE TOOLS FROM SUPERHARD MATERIALS | 2014 |
|
RU2588928C1 |
SOLDER FOR SOLDERING ALUMINIUM AND ALLOYS THEREOF | 2017 |
|
RU2661975C1 |
Authors
Dates
1997-08-20—Published
1979-11-29—Filed