FIELD: chemistry.
SUBSTANCE: electrolyte contains, g/l: chrome anhydride 70-100, sulphuric acid 0.7-1.0, indigo colourant 0.1-1.0, stroncium chloride 30-70. Electrolyte contains, g/l: chrome anhydride 70-100, sulphuric acid 0.7-1.0, indigo colourant 0.1-1.0, stroncium chloride 30-70, and at least one acid out of molybdic, vanadic, niobic, tantalic, tungstic, permanganic, technetic or rhenic acid 50-90.
EFFECT: enhanced microhardness and heat resistance of coatings, prolonged lifetime.
2 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF EXTRACTING MICROBIOLOGICAL SYNTHESIS LYSINE | 2008 |
|
RU2382823C2 |
ZINC ANODE FOR CHEMICAL CURRENT SOURCE | 2009 |
|
RU2406184C1 |
ELECTROLYTE FOR Cr-V ALLOY DEPOSITION | 2019 |
|
RU2713771C1 |
AIR ELECTRODE FOR CHEMICAL CURRENT SOURCE WITH OXYGEN REDUCTION ELECTROCATALYST | 2009 |
|
RU2419920C1 |
AIR ELECTRODE FOR CHEMICAL CURRENT SOURCE AND METHOD OF MAKING SAID ELECTRODE | 2008 |
|
RU2366039C1 |
GAS-DIFFUSION ELECTRODE OF CHEMICAL CURRENT SOURCE | 2009 |
|
RU2402115C1 |
PRIMARY AIR-ZINC CHEMICAL CURRENT SOURCE | 2009 |
|
RU2420835C1 |
ELECTROLYTE FOR PRODUCTION OF IRON-NICKEL ALLOYS | 2018 |
|
RU2694398C1 |
METHOD TO RECYCLE NICKEL-ZINC ALKALINE BATTERIES | 2011 |
|
RU2479078C2 |
METHOD OF ELECTRODEPOSITION OF CHROMIUM-MOLYBDENUM-DIAMOND COATINGS | 2020 |
|
RU2743133C1 |
Authors
Dates
2010-06-20—Published
2008-01-10—Filed