FIELD: process engineering.
SUBSTANCE: invention relates to powder metallurgy, particularly to production of composite materials. It can be used for production of strong wear-resistant parts, abrasive tools and sealing elements. Billet is produced by pressing the burden that comprises aluminium powder that features plate-like shape of particles and binder, and sintering in SHS-conditions. Sintered product is placed in mould, heated to 600÷775°C and 9÷12 MPa pressure is applied thereto for 1÷30 minutes to product deformation of 1.18÷1.25. Then product is cooled under pressure to 590÷650°C at the rated of 5÷10°C/min. Now, pressure is removed and product is cooled to ambient temperatures at the rate of 2.5÷4°/min.
EFFECT: high wear resistance, antifriction properties and resistance to propagation of fatigue cracks.
1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2015 |
|
RU2592917C1 |
METHOD OF PRODUCTION OF COMPOSITE MATERIAL AlO-Al | 2006 |
|
RU2319678C1 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2011 |
|
RU2461530C1 |
METHOD OF PRODUCING AlO-Al COMPOSITE MATERIAL | 2015 |
|
RU2583966C1 |
METHOD OF OBTAINING COMPOSITE MATERIAL Al-AlO | 2012 |
|
RU2521009C1 |
METHOD FOR PRODUCING ANTIFRICTION ALUMINIUM MATRIX COMPOSITE MATERIAL | 2022 |
|
RU2796870C1 |
METHOD OF OBTAINING A COMPOSITE MATERIAL AlO-Al | 2022 |
|
RU2799462C1 |
METHOD OF PRODUCING COMPOSITE MATERIAL AlO-Al | 2016 |
|
RU2632346C2 |
METHOD OF OBTAINING COMPOSITE MATERIAL AlO-Al | 2013 |
|
RU2545982C1 |
METHOD OF PRODUCTION OF COMPOSITE MATERIAL AlO-Al | 2004 |
|
RU2266270C1 |
Authors
Dates
2010-08-27—Published
2008-10-27—Filed