FIELD: metallurgy.
SUBSTANCE: procedure consists in preliminary modification of surface of polymer material and in successive application of metal layer. Preliminary modified surface of polymer material is performed by acceleration of particles of metal with a shock wave formed before front of detonation and in their penetration into surface of polymer material. A metal layer is applied on modified surface with flow of the said particles accelerated with products of detonation of gas mixture.
EFFECT: increased adhesion of metal to substrate and increased efficiency of process.
6 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SURFACE HARDENING OF A PART MADE OF POLYMER MATERIAL | 2021 |
|
RU2761191C1 |
METHOD FOR SURFACE HARDENING OF PARTS MADE OF POLYMERIC THERMOSETTING MATERIAL | 2022 |
|
RU2795315C1 |
METHOD FOR DETONATING APPLICATION OF COATINGS AND APPARATUS FOR IMPLEMENTING THEREOF | 2006 |
|
RU2329104C2 |
COATED PARTICLES | 2016 |
|
RU2697455C2 |
COATED PARTICLE | 2016 |
|
RU2697123C1 |
METHOD OF PRODUCING MICROWAVE ENERGY ABSORBING COATING | 2019 |
|
RU2712326C1 |
METHOD FOR APPLICATION OF COATINGS | 1993 |
|
RU2038411C1 |
METAL-BASED CATALYST CARRIER (OPTIONS) AND A METHOD FOR PREPARATION THEREOF (OPTIONS) | 2003 |
|
RU2234978C1 |
METHOD AND APPARATUS FOR APPLYING TITANIUM NITRIDE-BASED COATINGS | 2013 |
|
RU2566246C2 |
METHOD OF EXPLOSIVE APPLICATION OF COATING | 2007 |
|
RU2383655C2 |
Authors
Dates
2011-08-10—Published
2009-08-04—Filed