FIELD: chemistry.
SUBSTANCE: method involves preparation of a mixture from oil refining products, thermal oxidation and homogenisation. The mixture is prepared with preliminary thermal oxidation and homogenisation of the oil refining product - heavy pyrolysis resin - at temperature of 170-200°C in a hydropercussion-cavitation pulse emulsifier with treatment pulse frequency of 9500 rps for 3-4 hours; coal-tar pitch is then added in ratio of 1:1 and combined mixing is carried out at temperature of 200-250°C for 4-5 hours.
EFFECT: low consumption of coal-tar pitch as well as emissions of carcinogenic polycyclic aromatic hydrocarbons, the source of which is the coal-tar pitch.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING COAL TAR BINDER FOR ELECTRODE MATERIALS | 2012 |
|
RU2517502C1 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2015 |
|
RU2586139C1 |
METHOD FOR OBTAINING OIL-COAL TAR PITCH | 2014 |
|
RU2569355C1 |
METHOD OF PRODUCING PETROLEUM-AND-CARBON COAL BINDER | 2019 |
|
RU2729803C1 |
ANODE MASS FOR FORMING SELF-CALCINATING ANODE OF ALUMINIUM ELECTROLYTIC CELL | 2009 |
|
RU2397276C1 |
METHOD OF PRODUCING BINDER PITCH | 2014 |
|
RU2586135C1 |
INHIBITOR FOR ANODE MASS OF SELF-BAKING ANODE OF ALUMINIUM ELECTROLYSER | 2009 |
|
RU2415972C2 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2014 |
|
RU2582411C1 |
METHOD OF COMPOUND ELECTRODE PITCH PRODUCING FOR CARBON MATERIALS AND ARTICLES THEREFROM MAKING | 2015 |
|
RU2601766C1 |
METHOD OF PRODUCING OIL PITCH - COMPOSITE MATERIAL FOR PRODUCTION OF ANODE MASS | 2019 |
|
RU2722291C1 |
Authors
Dates
2013-08-10—Published
2012-03-12—Filed