FIELD: chemistry.
SUBSTANCE: method for producing complex cadmium oxide and iron of composition Cd1-xFexO, where 0.025≤x≤0.07 includes the preparation of a mixture of solutions of cadmium formate and iron formate in distilled water upon heating. The mixture is then evaporated to dry residue at 80-85°C in the air. The heat treatment of dry residue is carried out in two stages: stage I - at a temperature of 300-310°C for 0.5-0.6 hours and stage II at a temperature of 400-410°C for 2.0-2.5 hours.
EFFECT: producing a new chemical compound with high magnetization values at room temperature.
2 cl, 3 dwg, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING NANODISPERSE FERROMAGNETIC MATERIAL | 2014 |
|
RU2572123C2 |
METHOD OF MODIFICATION OF ALUMINUM POWDER | 2018 |
|
RU2679156C1 |
METHOD OF PRODUCING TUNGSTEN CARBIDE POWDER WITH COBALT BASED COATING | 2023 |
|
RU2813190C1 |
COMPLEX ALUMINUM AND RARE EARTH ELEMENTS OXIDE AND METHOD FOR ITS PRODUCTION | 2020 |
|
RU2746650C1 |
METHOD OF OBTAINING IRON FORMATE (II) | 2018 |
|
RU2670440C1 |
METHOD OF PRODUCING VANADYL FORMATE (IV) (EMBODIMENTS) | 2020 |
|
RU2732254C1 |
METHOD FOR OBTAINING AN OPTICAL SEMICONDUCTOR MATERIAL BASED ON NANODISPERSED CADMIUM OXIDE DOPED WITH LITHIUM | 2021 |
|
RU2754888C1 |
METHOD OF FABRICATING ZINC OXIDE NANOTUBES (VERSIONS) | 2010 |
|
RU2451579C2 |
THREE-LAYER SOLID ELECTROLYTE MEMBRANE OF MEDIUM TEMPERATURE SOFC | 2023 |
|
RU2812650C1 |
METHOD OF PRODUCING COPPER (II) FORMATE | 2019 |
|
RU2702227C1 |
Authors
Dates
2017-07-24—Published
2015-12-21—Filed