FIELD: metallurgy.
SUBSTANCE: slag-forming mixture is ground to a fraction of less than 0.001 mm, and the present refractory carbonates are removed by adding concentrated hydrochloric acid. Then pre-ground siderite (FeCO3) is added to the dried mixture in amount equal to the number of removed carbonates, the mixture is stirred, and the produced mixture is granulated. The replacement of refractory carbonates with iron carbonate in the composition prevents foaming of slag, which results in elimination of additional oxidation and carbonisation of steel and improvement of cast blank quality.
EFFECT: increased amount of siderite in slag creates conditions for secondary processing of slag with extraction of iron from it.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARATION TO PROCESSING OF SIDERITIC IRON ORE (VERSIONS) AND METHOD OF ITS FOLLOWING WASTE-FREE PROCESSING | 2011 |
|
RU2562016C1 |
SLAG FORMING COMPOSITION FOR STEEL CASTING | 2003 |
|
RU2245756C1 |
METHOD OF METAL AND SLAG HEAT ISOLATION IN NORMAL INGOT MAKING | 2008 |
|
RU2410190C2 |
METHOD OF USING CONSTRUCTION WASTES AS COMPONENT OF SLAG-FORMING MIXTURES | 2017 |
|
RU2677550C2 |
METHOD FOR SELECTIVE EXTRACTION OF METALS FROM COMPLEX ORES | 2011 |
|
RU2460813C1 |
SLAG-FREE FLUX FOR ADDITIVE PRODUCTION | 2016 |
|
RU2698239C2 |
"MELTING ON MELTING" METHOD FOR CONTINUOUS CASTING OF STEEL ONTO SLAB AND BLOOM BLANKS | 2006 |
|
RU2315680C2 |
METHOD FOR SELECTING SLAG COMPOSITION FOR EXTRACTION OF PLATINUM GROUP METALS FROM SPENT CATALYST USING IRON AS A COLLECTOR | 2021 |
|
RU2770393C1 |
POWDER WIRE FOR UNDERWATER WET CUTTING OF STEELS | 2020 |
|
RU2756005C1 |
SLAG FORMING MIXTURE FOR CONTINUOUS CASTING OF STEEL | 2018 |
|