FIELD: metallurgy. SUBSTANCE: method provides for hardening, heating up to 1000 C and after holding stepped ageing with cooling in furnace, respectively, at temperatures of 900 ± 20 C, with holding for 30-50 min, at 800 ± 20 C with holding for 80-100 min, at 700 ± 50 C with holding for 4-6 h, and at 600 ± 50 C with holding for 6-8 h and subsequent cooling in the air. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SOLDERING REFRACTORY DISPERSION-HARDENED NICKEL-CHROME BASE ALLOYS | 1996 |
|
RU2129061C1 |
BRAZING METHOD | 1995 |
|
RU2104840C1 |
PROCESS FOR MAKING DOUBLE-LAYER SOLDERED CONSTRUCTIONS | 1999 |
|
RU2169647C2 |
METHOD OF HEAT TREATMENT OF STRUCTURES | 1997 |
|
RU2129166C1 |
METHOD OF BRAZING OF TWO-LAYER CONSTRUCTIONS | 1995 |
|
RU2092286C1 |
METHOD OF THERMALLY TREATING WELDED JOINTS OF MARAGING STEELS | 1996 |
|
RU2103382C1 |
PROCESS FOR MAKING DOUBLE-LAYER SOLDERED CONSTRUCTIONS | 1999 |
|
RU2169646C2 |
TELESCOPIC STRUCTURE BRAZING METHOD | 1995 |
|
RU2104842C1 |
METHOD FOR MAKING DOUBLE-LAYER SOLDERED STRUCTURES | 2001 |
|
RU2226457C2 |
METHOD OF BRAZING OF TELESCOPIC ARTICLES MADE OF STEEL AND BRONZE | 1995 |
|
RU2104839C1 |
Authors
Dates
1998-02-20—Published
1995-04-21—Filed