FIELD: restoration of worn and strengthening of working surfaces of parts such as bodies of revolution.
SUBSTANCE: part is driven to rotation by means of rotation mechanism. Roller electrode is forced to part by means of loading mechanism and it rotates by action of friction force. Powder is fed from metering hopper to welding-on zone. When welding current pulse is absent powder is sucked to pipeline and it is fed to filter for collecting powder. If welding current pulse is supplied magnetic flux acts upon powder particles and powder particles are attracted under roller electrode for welding on to part. Powder excess is sucked to pipeline by effort less than attraction force of magnetic flux in welding on zone and it is fed to filter for collecting powder.
EFFECT: possibility for regulating quantity of sucked powder depending upon desired thickness of coating and modes of welding on, stable quality of welding on regardless wear degree of roller electrode.
1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
APPARATUS FOR ELECTRIC-CONTACT WELDING-ON OF FERROMAGNETIC POWDERS | 2006 |
|
RU2299795C1 |
ELECTRIC ARC SEAM WELDING OF FERROMAGNETIC POWDERS | 2010 |
|
RU2488467C2 |
DEVICE FOR ELECTRIC RESISTANCE WELDING OF FERROMAGNETIC POWDERS | 2007 |
|
RU2342233C2 |
METALLIC POWDER ELECTRIC-CONTACT WELDING-ON METHOD | 2006 |
|
RU2307010C1 |
DEVICE FOR SUPPLY OF FERROMAGNETIC POWDER IN ELECTROCONTACT WELDING | 2007 |
|
RU2340432C2 |
METHOD AND DEVICE FOR ELECTRIC CONTACT WELDING OF FERROMAGNETIC POWDER | 2010 |
|
RU2453407C2 |
DEVICE FOR ELECTRIC CONTACT WELDING OF FERROMAGNETIC POWDER | 2010 |
|
RU2428288C1 |
DEVICE FOR ELECTRIC-CONTACT WELDING OF FERROMAGNETIC POWDER | 2009 |
|
RU2415001C2 |
ELECTRIC ARC SEAM ROLLER WELDING OF METAL POWDERS | 2010 |
|
RU2564777C2 |
METHOD OF APPLYING COATING ON PART SURFACE BY ELECTRIC CONTACT WELDING USING POWDER FILLER CONTAINING IRON POWDER AND FILLER TO THIS END | 2011 |
|
RU2473413C2 |
Authors
Dates
2007-12-20—Published
2006-02-26—Filed