FIELD: machine building.
SUBSTANCE: protected surface of parts is prepared, a sublayer is applied, and chemical-thermal treatment of parts is carried out. The sublayer is applied from silicon or powdery metals from a group of transition metals, or metals of chrome subgroup with the help of plasma sputtering. Chemical-thermal treatment of the sublayer is carried out in a powder-type layer containing an active powder mixture at the following ratio of reagents, wt %: ammonium chloride not more than 5, titanium or aluminium or nickel 39-50, aluminium oxide and/or titanium diboride 4-55, carbon or boron, or silicon, or silicon carbide - balance. Saturation of the sublayer with the active powder mixture is carried out under vacuum or in a protective medium from inert gas under thermal treatment for 1-4 hours at the temperature in the range of 800-1100°C.
EFFECT: improved quality of a coating due to its increased thermal resistance, chemical resistance and mechanical strength.
2 dwg, 2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR APPLYING A PROTECTIVE COATING ON STEEL | 2021 |
|
RU2763130C1 |
METHOD FOR OBTAINING OF PROTECTIVE COAT ON ALLOYS | 2002 |
|
RU2232206C1 |
METHOD OF HARDENING PARTS MADE FROM CONSTRUCTION AND TOOL STEELS | 2007 |
|
RU2345175C1 |
STRENGTHENING METHOD OF STEEL PARTS | 2008 |
|
RU2381299C1 |
HIGH-TEMPERATURE ANTI-OXIDATION COATING | 2022 |
|
RU2800358C1 |
METHOD FOR FORMATION OF PROTECTIVE COATINGS ON ALLOYS | 1994 |
|
RU2073742C1 |
PROCEDURE OF APPLICATION OF PROTECTIVE COATING ON PARTS OUT OF NICKEL ALLOYS | 2008 |
|
RU2375497C1 |
MATERIAL FOR HEAT-RESISTANT PROTECTIVE COATING | 2017 |
|
RU2685905C1 |
METHOD FOR APPLICATION OF CERAMIC COATING ONTO PARTS FROM CAST IRON AND STEEL | 2011 |
|
RU2482215C1 |
POWDER CHARGE AND METHOD TO PRODUCE OUT OF IT PROTECTIVE METAL-CERAMIC COATING ON PIECES OF DISPERSION-HARDENING NICKLE ALLOYS | 1994 |
|